Browsing by Subject "nanoindentation"
Now showing items 1-2 of 2
-
ATOMISTIC SIMULATION STUDY OF THE EFFECTS OF POINT DEFECTS ON THE INCEPTION OF PLASTIC DEFORMATION IN METALS
(2013)Atomistic simulations have been used to study the effect of various types of point defects on the mechanical response of FCC single crystals in nanoindentation and uniaxial tests. To study the effect of spatial distribution ... -
ATOMISTIC STUDIES OF DEFORMATION MECHANISMS IN NANOSCALE MULTILAYERED METALLIC COMPOSITES
(2010)The goal of this thesis is to understand the interaction between dislocations and various metallic interfaces in nanoscale metallic multilayers (NMM). At lower strain rates, this mean understanding the effect of interfaces ...